Yesterday I had a chance to pour the main area of the heat blanket. I cured it with out any pressure on it and so unfortunately it picks up a few wrinkles from the protective plastic I laid down on the work surface. However, it only has 660gm of rubber in it so I have some left over to try to remedy it.
Check out all the details on the Equipment Forum here. Construction details